Below you will find a selection of photographs of typical problems with pipeline coatings...
Blistering of FBE joint field coating
Corrosion under a 3 year old 3 Layer PE coating
Foaming of an FBE coating
Heat shrink failure
Lack of wetting and flow of FBE layer
Under cutting of a stored 3LPP coating
3LPE coating showing loss of adhesion of FBE (1st layer) to steel substrate, before ditching
Voids under the FBE (1st layer) of a 3LPE coating, before ditching
David Norman Corrosion Control Glynn Heath, West Pentire Road, Crantock, Cornwall, TR8 5SA, England. Tel: + 44 1637 830 915 - Fax: +44 1637 830 863 - Email: click here